Curie temperature and working temperature of sintered NdFeB

Different product grades of sintered NdFeB have different properties. In short, the number represents the maximum magnetic energy product of the product. The larger the number, the greater the maximum magnetic energy product; the letter after the number represents the classification of its intrinsic coercivity, and the backward the brand, the greater the intrinsic coercivity.

20201231014930 80989 - Curie temperature and working temperature of sintered NdFeB

After understanding the sintered NdFeB grades, everyone will definitely ask: What is the relationship between temperature and the magnetic properties of NdFeB products? Is the working temperature of different brands of products the same? What is the upper limit of heat-resistant working temperature? Today, yueci will introduce the working temperature of sintered NdFeB.

When it comes to the relationship between temperature and magnetism, we must first understand a concept-“Curie temperature”. Does it feel familiar to hear the word Curie? Did you think of the famous madame curie? This concept is barely related to madame curie.

  • More than 200 years ago, a famous physicist discovered a physical property of magnets in his laboratory, that is, when a magnet is heated to a certain temperature, its original magnetism will disappear. This great physicist is Mrs. Li’s husband, Pierre Curie, later people called this temperature Curie point (Curie point), also called Curie temperature (Tc) or magnetic transition point.
  • Definition: The Curie temperature is the temperature at which a magnetic material changes between a ferromagnetic body and a paramagnetic body. When the temperature is lower than the Curie temperature, the substance becomes a ferromagnetic body. At this time, the magnetic field related to the material is difficult to change. When the temperature is higher than the Curie temperature, the substance becomes a paramagnetic body, and the magnetic field of the magnet can easily change with the surrounding magnetic field.
  • Value: Curie temperature represents the theoretical working temperature limit of magnetic materials. The Curie temperature of NdFeB is 320-380 °C. The level of the Curie point is related to the crystal structure formed by the sintering of the magnet.
  • What happens if the Curie temperature is exceeded? If the temperature reaches the Curie temperature, the molecules inside the magnet move violently and demagnetize, which is irreversible.

After talking about the Curie temperature, let’s talk about the working temperature (Tw). In fact, the Curie temperature is only the temperature under laboratory conditions, or it can be said to be the ideal temperature, and the working temperature of the magnet is the material. The maximum temperature for maintaining magnetism in actual situations. The maximum working temperature of sintered NdFeB is much lower than its Curie temperature. In the working temperature, the magnetic force will decrease when the temperature rises, but most of the magnetic force will recover after cooling down.

  • The relationship between working temperature and Curie temperature: The higher the Curie temperature, the higher the working temperature of the magnetic material, and the better the temperature stability. Adding cobalt, terbium, dysprosium and other elements to the sintered neodymium iron boron raw material can increase its Curie temperature.
  • The maximum operating temperature of sintered NdFeB depends on its own magnetic properties and the selection of operating points. For the same sintered NdFeB magnet, the closer the working magnetic circuit is, the higher the maximum use temperature of the magnet and the more stable the performance of the magnet. Therefore, the maximum operating temperature of the magnet is not a certain value, but changes with the degree of closure of the magnetic circuit. Under the premise of a given operating point, the maximum operating temperature and Curie temperature of each grade of sintered NdFeB magnet are as follows:

Thermal Characteristics of Sintered NdFeB Magnets

Neodymium Material Type Maximum Operating Temp Curie Temp
N 176°F (80°C) 590°F (310°C)
M 212°F (100°C) 644°F (340°C)
H 248°F (120°C) 644°F (340°C)
SH 302°F (150°C) 644°F (340°C)
UH 356°F (180°C) 662°F (350°C)
EH 392°F (200°C) 662°F (350°C)
AH 428°F (220°C) 662°F (350°C)

Source: China Permanent Magnet Manufacturer – www.ymagnet.com

Summary
curie temperature and working temperature of sintered ndfeb - Curie temperature and working temperature of sintered NdFeB
Article Name
Curie temperature and working temperature of sintered NdFeB
Description
In fact, the Curie temperature is only the temperature under laboratory conditions, or it can be said to be the ideal temperature, and the working temperature of the magnet is the material.
Author
Publisher Name
www.ymagnet.com
Publisher Logo
PREV
NEXT

RELATED POSTS

Leave a Reply

*

*

Inquery now

SUBSCRIBE TO OUR NEWSLETTER

FOLLOW US

العربية简体中文繁體中文NederlandsEnglishFrançaisDeutschItaliano日本語한국어PortuguêsРусскийEspañolไทย

Email me
Mail to us